Community / Article

1.1321 — alloy Steel: Composition, Properties & Applications

Aug 23, 2026 0 views 0 comments
Also known as: 1.1321
EN/DIN steel grade 1.1321

CHEMICAL COMPOSITION
C:0.10-0.25;Si:0.10-0.40;Mn:0.30-1.50;Cr:0.30-1.20;P:≤0.035;S:≤0.035

TYPICAL APPLICATIONS
General engineering and manufacturing use per EN/DIN specification.

AVAILABLE FORMS
Bar, plate, sheet, tube, forgings, strip, wire

HEAT TREATMENT
Typically normalized (880–920 °C, air cool) or carburized (900–930 °C) for case-hardening grades, then quenched and tempered at 150–200 °C. Carburize 900–930 °C, direct/intake quench, temper 150–200 °C; useful case depth 0.5–1.5 mm.

PROCESSING PRECAUTIONS
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating). Machine the core stock before surface hardening; leave grinding allowance for the hardened case.

SOURCE & SUPPLY
Shanxi Youte Steel stocks 1.1321 in bars, plates, pipes and forgings with mill test certificates, cut-to-length service and export packaging. Contact our team for quotations and technical data sheets.
Share this article

0 Comments

No comments yet. Be the first to share your thoughts!

Leave a Comment

Online / AI
AI
XiaoGang · AI Steel Expert
JLHSteel · 7×24 Online
Quick: 304 vs 316L Food-grade steel Carbon vs alloy steel High-strength steel Inquiry tips