1.0472 — alloy Steel: Composition, Properties & Applications

Aug 23, 2026 0 views 0 comments
Also known as: 1.0472
EN/DIN steel grade 1.0472

CHEMICAL COMPOSITION
C:0.05-0.70;Si:0.10-0.50;Mn:0.30-1.60;P:≤0.045;S:≤0.045

TYPICAL APPLICATIONS
General engineering and manufacturing use per EN/DIN specification.

AVAILABLE FORMS
Bar, plate, sheet, tube, forgings, strip, wire

HEAT TREATMENT
Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.

PROCESSING PRECAUTIONS
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).

SOURCE & SUPPLY
Shanxi Youte Steel stocks 1.0472 in bars, plates, pipes and forgings with mill test certificates, cut-to-length service and export packaging. Contact our team for quotations and technical data sheets.
Share this article

0 Comments

No comments yet. Be the first to share your thoughts!

Leave a Comment

Online / AI
AI
XiaoGang · AI Steel Expert
JLHSteel · 7×24 Online
Quick: 304 vs 316L Food-grade steel Carbon vs alloy steel High-strength steel Inquiry tips