Community / Article

06Cr25Ni20Si2 — stainless Steel: Composition, Properties & Applications

Aug 23, 2026 0 views 0 comments
Also known as: 06Cr25Ni20Si2
25Cr-20Ni austenitic, high-temp oxidation resistant. (GB/T 20878; equiv ASTM 310S / EN 1.4841 / JIS SUS310S). Nominal values—confirm mill certificate.

CHEMICAL COMPOSITION
C:≤0.08;Cr:24.0-26.0;Ni:19.0-22.0

MECHANICAL PROPERTIES
Tensile:≥515 MPa;Yield:≥205 MPa;Elong:≥40%

TYPICAL APPLICATIONS
25Cr-20Ni,耐高温氧化。,"Plate

AVAILABLE FORMS
Bar"

STANDARDS & EQUIVALENT GRADES
T 20878 06Cr25Ni20Si2; ASTM 310S; EN 1.4841 / JIS SUS310S

HEAT TREATMENT
Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).

PROCESSING PRECAUTIONS
Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.

SOURCE & SUPPLY
Shanxi Youte Steel stocks 06Cr25Ni20Si2 in bars, plates, pipes and forgings with mill test certificates, cut-to-length service and export packaging. Contact our team for quotations and technical data sheets.
Share this article

0 Comments

No comments yet. Be the first to share your thoughts!

Leave a Comment

Online / AI
AI
XiaoGang · AI Steel Expert
JLHSteel · 7×24 Online
Quick: 304 vs 316L Food-grade steel Carbon vs alloy steel High-strength steel Inquiry tips