| Element | Content |
|---|---|
| Ni | -base: C 0.05 max Cr 24.0-27.0 Ni 44.0-47.0 Co 2.5-4.0 Mo 2.5-4.0 W 2.5-4.0 Fe 15.0-19.0 |
High-temperature alloy; typical Tensile 700-1400 MPa, Yield 400-1100 MPa at room temp; retains strength to 650-870 C (grade/heat-treat dependent)