| Element | Content |
|---|---|
| Fe | -base: C 0.36-0.46 Cr 19.0-21.0 Ni 19.0-21.0 Co 19.0-21.0 Mo 3.5-4.5 W 3.5-4.5 Nb 3.5-4.5 Fe bal |
High-temperature alloy; typical Tensile 700-1400 MPa, Yield 400-1100 MPa at room temp; retains strength to 650-870 C (grade/heat-treat dependent)