S12C
S12C · alloy
S12C
Bar,Plate | JIS G4051 S12C
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
S130
S130 · alloy
S130
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S130
S1300MC · alloy
S1300MC
Plate,Section | EN 10025
C:0.10-0.20;Si:0.15-0.40;Mn:0.60-1.00;P:≤0.035;S:≤0.035
S131
S131 · alloy
S131
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S132
S132 · alloy
S132
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S133
S133 · alloy
S133
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S134
S134 · alloy
S134
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S135
S135 · alloy
S135
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap |
C:0.28-0.33;Si:0.15-0.35;Mn:0.40-0.60;Cr:0.80-1.10;Mo:0.15-0.25
S136
S136 · other
S136 / 1.2083
Block,Round | AISI 420 Modified
C:0.36-0.42;Si:≤1.00;Mn:≤1.00;Cr:13.0-14.5;P:≤0.030;S:≤0.030
S137
S137 · alloy
S137
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S138
S138 · alloy
S138
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S139
S139 · alloy
S139
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S13C
S13Cr-110 · stainless
S13Cr-110
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈5%) stabilises the austenite and improves toughness and pitting resistance. Molybdenum (≈2%) enhances resistance | 改型13Cr
C:≤0.03;Cr:12.0-14.5;Ni:3.5-6.5;Mo:1.5-2.5;V:0.05-0.10
S13C
S13Cr-95 · stainless
S13Cr-95
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈5%) stabilises the austenite and improves toughness and pitting resistance. Molybdenum (≈2%) enhances resistance | 改型13Cr
C:≤0.03;Cr:12.0-14.5;Ni:3.5-6.5;Mo:1.5-2.5;V:0.05-0.10
S140
S140 · alloy
S140
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S141
S141 · alloy
S141
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S142
S142 · alloy
S142
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S143
S143 · alloy
S143
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040
S144
S144 · alloy
S144
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.10-0.50;Mn:0.40-1.60;Si:0.10-0.50;P:≤0.040;S:≤0.040