SY29
SY295 · alloy
SY295
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.05-0.60;Si:0.10-2.50;Mn:0.30-2.50;Cr:0.00-2.00;Ni:0.00-4.50;Mo:0.00-1.00;P:≤0.040;S:≤0.040
SY39
SY390 · alloy
SY390
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.05-0.60;Si:0.10-2.50;Mn:0.30-2.50;Cr:0.00-2.00;Ni:0.00-4.50;Mo:0.00-1.00;P:≤0.040;S:≤0.040
SYQ-
SYQ-01 · alloy
SYQ-01
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-01
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-02 · alloy
SYQ-02
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-02
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-03 · alloy
SYQ-03
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-03
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-05 · alloy
SYQ-05
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-05
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-08 · alloy
SYQ-08
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-08
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-13Cr · alloy
SYQ-13Cr
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-13Cr
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-13Cr-110 · alloy
SYQ-13Cr-110
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-13Cr-110
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-13Cr-95 · alloy
SYQ-13Cr-95
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-13Cr-95
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-2205 · alloy
SYQ-2205
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-2205
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-2507 · alloy
SYQ-2507
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-2507
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-L80 · alloy
SYQ-L80
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-L80
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-N80 · alloy
SYQ-N80
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-N80
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYQ-
SYQ-P110 · alloy
SYQ-P110
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-P110
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYW2
SYW295 · alloy
SYW295
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.05-0.60;Si:0.10-2.50;Mn:0.30-2.50;Cr:0.00-2.00;Ni:0.00-4.50;Mo:0.00-1.00;P:≤0.040;S:≤0.040
SYW3
SYW390 · alloy
SYW390
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.05-0.60;Si:0.10-2.50;Mn:0.30-2.50;Cr:0.00-2.00;Ni:0.00-4.50;Mo:0.00-1.00;P:≤0.040;S:≤0.040
T001
T00103 · toolsteel
T00103
| ASTM A686
C 1.00-1.10, Mn 0.10-0.40, Si 0.10-0.40
T054
T05401 (GB Stainless Mo-Series Hot-Rolled Bar) · stainless
GB Stainless Mo-Series Hot-Rolled Bar
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0