T379
T37993 (GB Stainless Mo-Series Hot-Rolled Sheet Size 5) · stainless
GB Stainless Mo-Series Hot-Rolled Sheet Size 5
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0
T379
T37994 (GB Stainless Mo-Series Normalized Tube Size 5) · stainless
GB Stainless Mo-Series Normalized Tube Size 5
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0
T379
T37995 (GB Stainless Mo-Series Annealed Pipe Size 5) · stainless
GB Stainless Mo-Series Annealed Pipe Size 5
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0
T379
T37996 (GB Stainless Mo-Series Quenched & Tempered Forging Size 5) · stainless
GB Stainless Mo-Series Quenched & Tempered Forging Size 5
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0
T379
T37997 (GB Stainless Mo-Series Normalized & Tempered Rod Size 5) · stainless
GB Stainless Mo-Series Normalized & Tempered Rod Size 5
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0
T379
T37998 (GB Stainless Mo-Series Cold-Drawn Wire Size 5) · stainless
GB Stainless Mo-Series Cold-Drawn Wire Size 5
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0
T379
T37999 (GB Stainless Mo-Series Stress-Relieved Block Size 5) · stainless
GB Stainless Mo-Series Stress-Relieved Block Size 5
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0
T380
T38000 (GB Stainless Mo-Series Hardened & Tempered Strip Size 5) · stainless
GB Stainless Mo-Series Hardened & Tempered Strip Size 5
| GB/T 20878
C:≤0.08;Cr:16.0-18.0;Mn:≤2.00;Mo:2.00-3.00;Ni:10.0-14.0
T4
T4 · other
T4
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈5%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy syste | ASTM A600 T4
C:0.70-0.80;W:17.0-19.0;Cr:3.75-4.50;V:0.80-1.20;Co:4.25-5.75;P:≤0.030;S:≤0.030
T5
T5 · other
T5
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈8.25%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy sy | ASTM A600 T5, ASME SA-213 / SA-213M; ASTM A213, ASTM A250 / A250M
C:0.75-0.85;W:17.0-19.0;Cr:3.75-4.50;V:1.80-2.30;Co:7.00-9.50;P:≤0.030;S:≤0.030
T5b
T5b · alloy
T5b
Bar,Plate | ASTM A213 T5b, ASME SA-213 / SA-213M; ASTM A213
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T5c
T5c · alloy
T5c
| ASME SA-213 / SA-213M
C 0.15 max Si 1.00-2.00 Mn 0.30-0.60 P 0.025 S 0.025 Cr 4.00-6.00 Mo 0.45-0.65
T6
T6 · other
T6
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈12%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy syst | ASTM A600 T6
C:0.72-0.82;W:18.0-21.0;Cr:3.75-4.50;V:2.40-2.80;Co:11.0-13.0;P:≤0.030;S:≤0.030
T60
T60 · alloy
T60
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T65-
T65-40 · other
T65-40
| ASTM A463 / A463M
C 0.20 max Mn 1.35 max (Type 2 high-tensile); Al-Si coating
T65-
T65-50 · other
T65-50
| ASTM A463 / A463M
C 0.20 max Mn 1.35 max; Al-Si coating
T65-
T65-60 · other
T65-60
| ASTM A463 / A463M
C 0.20 max Mn 1.35 max; Al-Si coating
T7
T7 · alloy
T7
Bar,Plate | ASTM A213 T7, ASME SA-213 / SA-213M; ASTM A213
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T75
T75 · alloy
T75
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040