WJX
WJX 770 · alloy
WJX 770
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.04-0.40;Si:0.10-0.60;Mn:0.40-2.50;Nb:0.00-0.10;Ti:0.00-0.20;P:≤0.030;S:≤0.020
WJX
WJX 780 · alloy
WJX 780
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.04-0.40;Si:0.10-0.60;Mn:0.40-2.50;Nb:0.00-0.10;Ti:0.00-0.20;P:≤0.030;S:≤0.020
WJX
WJX 790 · alloy
WJX 790
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.04-0.40;Si:0.10-0.60;Mn:0.40-2.50;Nb:0.00-0.10;Ti:0.00-0.20;P:≤0.030;S:≤0.020
WQS-
WQS-01 · alloy
WQS-01
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
WQS-
WQS-02 · alloy
WQS-02
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
WQS-
WQS-03 · alloy
WQS-03
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
WQS-
WQS-05 · alloy
WQS-05
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
WQS-
WQS-08 · alloy
WQS-08
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
WQS-
WQS-10 · alloy
WQS-10
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
WQS-
WQS-15 · alloy
WQS-15
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
WQS-
WQS-20 · alloy
WQS-20
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
X-40
X-40 · alloy
X-40
Bar,Rod,Powder |
Co:balance;Cr:28.0-32.0;W:3.5-5.5;C:1.0-1.4;Si:≤2.0;Mn:≤1.0;Fe:≤3.0
X-45
X-45 · alloy
X-45
Bar,Rod,Powder |
Co:balance;Cr:28.0-32.0;W:3.5-5.5;C:1.0-1.4;Si:≤2.0;Mn:≤1.0;Fe:≤3.0
X-95
X-95 · alloy
X-95
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | X-95 / API X-grade
C:0.28-0.33;Si:0.15-0.35;Mn:0.40-0.60;Cr:0.80-1.10;Mo:0.15-0.25
X066
X06601 (Case-Hardening Steels Hot-Rolled Bar) · alloy
Case-Hardening Steels Hot-Rolled Bar
| AISI/SAE
C:0.18-0.23;Cr:0.40-0.60;Mn:0.60-0.95;Mo:0.15-0.25;Ni:0.40-0.70
X066
X06602 (Case-Hardening Steels Normalized Plate) · alloy
Case-Hardening Steels Normalized Plate
| AISI/SAE
C:0.18-0.23;Cr:0.40-0.60;Mn:0.60-0.95;Mo:0.15-0.25;Ni:0.40-0.70
X066
X06603 (Case-Hardening Steels Annealed Sheet) · alloy
Case-Hardening Steels Annealed Sheet
| AISI/SAE
C:0.18-0.23;Cr:0.40-0.60;Mn:0.60-0.95;Mo:0.15-0.25;Ni:0.40-0.70
X066
X06604 (Case-Hardening Steels Quenched & Tempered Tube) · alloy
Case-Hardening Steels Quenched & Tempered Tube
| AISI/SAE
C:0.18-0.23;Cr:0.40-0.60;Mn:0.60-0.95;Mo:0.15-0.25;Ni:0.40-0.70
X066
X06605 (Case-Hardening Steels Normalized & Tempered Pipe) · alloy
Case-Hardening Steels Normalized & Tempered Pipe
| AISI/SAE
C:0.18-0.23;Cr:0.40-0.60;Mn:0.60-0.95;Mo:0.15-0.25;Ni:0.40-0.70