ШХ21

Alloy Steel

ШХ21

Russian GOST bearing steel.

Chemical Composition (%)

C0.95
SI0.3
MN1.1
CR1.3
P0.027
S0.02

Applications

International high-end steel grade for aerospace, oil & gas, defense or engineering machinery.

Available Forms

Bar, plate, sheet, tube, forgings, strip, wire, powder

Uses

High-carbon chromium bearing steel for rolling-element bearings, races and precision balls/rollers. Combines high hardness, fatigue life and dimensional stability; also used for gauges, needles and wear parts.

Heat Treatment

Spheroidize anneal (760–780 °C), austenitize 830–860 °C oil quench, temper 150–180 °C to 60–66 HRC; stabilising treatments improve dimensional stability.

Precautions

Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).