ЭИ1466
High-Temp SteelЭИ1466
Russian GOST heat-resistant special steel EI1466.
Chemical Composition (%)
| C | 0.15 |
|---|---|
| SI | 1 |
| MN | 1.5 |
| CR | 15 |
| NI | 24 |
| P | 0.03 |
| S | 0.02 |
Applications
International high-end steel for aerospace, oil & gas, defense or engineering.
Available Forms
Bar, plate, sheet, tube, forgings, strip, wire, powder
Uses
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.
Heat Treatment
Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.
Precautions
Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.