00Cr18Ni5Mo3Si2
Stainless Steel00Cr18Ni5Mo3Si2
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. Used in food processing, chemical plant, architecture, heat exchangers,
Chemical Composition (%)
| C | 0.03 |
|---|---|
| SI | 1.3 |
| MN | 1 |
| CR | 18 |
| NI | 4.5 |
| MO | 2.5 |
| P | 0.035 |
| S | 0.03 |
Applications
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. Used in food processing, chemic
Available Forms
Bar, plate, forgings, tube
Uses
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.
Heat Treatment
Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).
Precautions
Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.