00Cr25Ni22Mo2N

Stainless Steel

00Cr25Ni22Mo2N / 奥,

Applications

Sheet, Plate, Bar, Tube, Pipe

Available Forms

Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈23%) stabilises the austenite and improves toughness and pitting resistance. Molybdenum (≈2.1%) enhances resistance to chloride pitting and crevice corrosion — suited to marine and chemical service. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.

Uses

Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).

Heat Treatment

Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.