022Cr11Ti

Stainless Steel

022Cr11Ti

Automotive exhaust ferritic stainless. (GB/T 20878; equiv ASTM 409 / EN 1.4512 / JIS SUS409). Nominal values—confirm mill certificate.

Chemical Composition (%)

C0.08
CR10.5
TI6

Mechanical Properties

Tensile:≥380 MPa;Yield:≥170 MPa

Chinese Standard

T 20878 022Cr11Ti

Equivalent Standards

ASTM 409

Equivalent Grades

EN 1.4512 / JIS SUS409

Applications

汽车排气用铁素体。,"Sheet

Available Forms

Tube"

Uses

Ferritic stainless steel with good resistance to stress-corrosion cracking and oxidation, plus formability and lower cost. Used for automotive trim, exhaust systems, domestic appliances, decorative and welded structures.

Heat Treatment

Annealed at 780–850 °C and air cooled; stabilize at 600–800 °C to avoid 475 °C embrittlement; not hardenable by heat treatment.

Precautions

Avoid welding in the 475 °C embrittlement and sigma-phase ranges; use matched filler and minimize heat input. Good resistance to stress-corrosion cracking.