022Cr17Ni12Mo2Ti
Stainless Steel022Cr17Ni12Mo2Ti
High-Mo austenitic, enhanced corrosion resistance. (GB/T 20878; equiv ASTM 317 / JIS SUS317). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.08 |
|---|---|
| CR | 18 |
| NI | 11 |
| MO | 3 |
Mechanical Properties
Tensile:≥515 MPa;Yield:≥205 MPa
Chinese Standard
T 20878 022Cr17Ni12Mo2Ti
Equivalent Standards
ASTM 317
Equivalent Grades
JIS SUS317
Applications
高钼奥氏体,耐蚀更强。,"Plate
Available Forms
Bar"
Uses
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈13%) stabilises the austenite and improves toughness and pitting resistance. Molybdenum (≈3.5%) enhances resistance to chloride pitting and crevice corrosion — suited to marine and chemical service. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.
Heat Treatment
Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).
Precautions
Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.