06Cr25Ni20
Stainless Steel06Cr25Ni20
25Cr-20Ni austenitic, high-temp oxidation resistant. (GB/T 20878; equiv ASTM 310S / EN 1.4841 / JIS SUS310S). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.08 |
|---|---|
| SI | 1 |
| MN | 2 |
| P | 0.045 |
| S | 0.03 |
| CR | 24 |
| NI | 19 |
Mechanical Properties
Tensile:≥515 MPa;Yield:≥205 MPa;Elong:≥40%
Chinese Standard
T 20878 06Cr25Ni20
Equivalent Standards
ASTM 310S
Equivalent Grades
EN 1.4841 / JIS SUS310S
Applications
25Cr-20Ni,耐高温氧化。,"Plate
Available Forms
Bar"
Uses
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈20.5%) stabilises the austenite and improves toughness and pitting resistance. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.
Heat Treatment
Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).
Precautions
Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.