07Cr2AlMoRe
Alloy Steel07Cr2AlMoRe
Boiler tube, main steam pipe. (GB 5310; equiv GB 5310 12Cr1MoVG / T12). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.08 |
|---|---|
| CR | 0.9 |
| MO | 0.25 |
| V | 0.15 |
Mechanical Properties
Tensile:≥470 MPa;Yield:≥255 MPa
Chinese Standard
GB 5310 07Cr2AlMoRe
Equivalent Standards
GB 5310 12Cr1MoVG / T12
Applications
锅炉管,主蒸汽管。,Tube
Available Forms
Carburizing (case-hardening) steel with low carbon core for toughness and a hard, wear-resistant surface after carburizing. Used for gears, camshafts, pinions, spline shafts, bushings and transmission parts subjected to fatigue and surface wear.
Uses
Typically normalized (880–920 °C, air cool) or carburized (900–930 °C) for case-hardening grades, then quenched and tempered at 150–200 °C. Carburize 900–930 °C, direct/intake quench, temper 150–200 °C; useful case depth 0.5–1.5 mm.
Heat Treatment
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating). Machine the core stock before surface hardening; leave grinding allowance for the hardened case.
Comments 0