08Х17
Stainless Steel08Х17
Russian GOST ferritic stainless.
Chemical Composition (%)
| C | 0.08 |
|---|---|
| SI | 0.8 |
| MN | 2 |
| CR | 16 |
| P | 0.035 |
| S | 0.025 |
Applications
International high-end steel for aerospace, oil & gas, defense or engineering.
Available Forms
Bar, plate, sheet, tube, forgings, strip, wire, powder
Uses
Ferritic stainless steel with good resistance to stress-corrosion cracking and oxidation, plus formability and lower cost. Used for automotive trim, exhaust systems, domestic appliances, decorative and welded structures.
Heat Treatment
Annealed at 780–850 °C and air cooled; stabilize at 600–800 °C to avoid 475 °C embrittlement; not hardenable by heat treatment.
Precautions
Avoid welding in the 475 °C embrittlement and sigma-phase ranges; use matched filler and minimize heat input. Good resistance to stress-corrosion cracking.