Alloy Steel08X15H24V4TR
(GOST 5632). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.05 |
|---|---|
| V | 3.4 |
| P | 0.035 |
| S | 0.035 |
Mechanical Properties
Tensile:≥510 MPa;Yield:≥295 MPa;Elong:≥20%
Chinese Standard
GOST 5632 08X15H24V4TR
Available Forms
Bar,Plate
Uses
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Vanadium (≈4%) refines grain and strengthens the tempered structure. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.
Heat Treatment
Typically normalized (880–920 °C, air cool) or carburized (900–930 °C) for case-hardening grades, then quenched and tempered at 150–200 °C.
Precautions
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).