0Cr18Ni12Mo2Ti

Stainless Steel

0Cr18Ni12Mo2Ti

Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. Used in food processing, chemical plant, architecture, heat exchangers,

Chemical Composition (%)

C0.08
SI1
MN2
CR16
NI11
MO1.8
TI5
P0.035
S0.03

Applications

Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. Used in food processing, chemic

Available Forms

Bar, plate, forgings, tube

Uses

Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.

Heat Treatment

Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).

Precautions

Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.