0Cr26Ni5Mo2Cu3Ti

Stainless Steel

0Cr26Ni5Mo2Cu3Ti

Early duplex stainless steel. (GB/T 20878; equiv UNS S32900 / JIS SUS329J1). Nominal values—confirm mill certificate.

Chemical Composition (%)

C0.08
CR23
NI2.5
MO1

Mechanical Properties

Tensile:≥640 MPa;Yield:≥440 MPa

Chinese Standard

T 20878 0Cr26Ni5Mo2Cu3Ti

Equivalent Grades

UNS S32900 / JIS SUS329J1

Applications

早期双相不锈钢。,"Plate

Available Forms

Tube"

Uses

Ferritic stainless steel with good resistance to stress-corrosion cracking and oxidation, plus formability and lower cost. Used for automotive trim, exhaust systems, domestic appliances, decorative and welded structures.

Heat Treatment

Annealed at 780–850 °C and air cooled; stabilize at 600–800 °C to avoid 475 °C embrittlement; not hardenable by heat treatment.

Precautions

Avoid welding in the 475 °C embrittlement and sigma-phase ranges; use matched filler and minimize heat input. Good resistance to stress-corrosion cracking.