1.1169
Alloy Steel1.1169
1.1169 supplied by Shanxi Youte Steel (jlhsteel.net).
Chemical Composition (%)
| C | 0.6 |
|---|---|
| MN | 0.5 |
| SI | 0.4 |
Chinese Standard
EN 10083-1
Equivalent Grades
Ck67 / AISI 1065
Available Forms
Bar, Plate, Tube, Forging, Wire
Uses
High-carbon grade for rails, springs, cutting tools, wear plates and components demanding high hardness and wear resistance after heat treatment. Commonly supplied as bar, plate, sheet, tube and forging.
Heat Treatment
Austenitize at 760–820 °C and quench (oil/water) then temper at 150–400 °C for high hardness; spheroidize anneal (680–720 °C) improves machinability of the as-rolled bar.
Precautions
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).