1.2344 ESR

Other

1.2344 ESR (H13)

Premium ESR-refined H13 hot work tool steel. Maximized isotropy & toughness.

Chemical Composition (%)

C0.37
SI0.9
MN0.3
CR4.8
MO1.2
V0.9
P0.015
S0.003

Mechanical Properties

Hardness(annealed):≤229 HB;Hardness(hardened):48-55 HRC

Chinese Standard

DIN 1.2344 ESR

Equivalent Grades

Premium H13 ESR

Applications

Premium die casting, hot stamping, extrusion

Available Forms

Round,Block

Uses

Tool and die steel for cutting, forming, punching and molding tools. Tungsten/molybdenum (≈0%/1.35%) give hot hardness and red-hardness for high-speed and hot-work tools. High chromium (≈5.15%) provides wear resistance and secondary hardening. Applied to blanks, punches, extrusion dies, shear blades, plastic-mold and cold-work tooling.

Heat Treatment

Hot-work: preheat 800 °C, austenitize 1020–1080 °C, quench, temper 540–620 °C (multiple) for hot hardness and thermal fatigue resistance.

Precautions

Risk of quench cracking and distortion — use graded preheating, controlled cooling and multiple tempers. Avoid overheating the austenitizing temperature. Machine in the soft annealed condition; allow for dimensional change after heat treatment. Grind with coolant to prevent rehardening cracks.