1.4216

Stainless Steel

1.4216

DIN stainless steel grade 1.4216 (X-series corrosion-resistant).

Chemical Composition (%)

C0.12
SI1
MN1
CR16
P0.04
S0.03

Mechanical Properties

Tensile:≥520 MPa;Yield:≥210 MPa;Elongation:≥40%

Equivalent Standards

EN equivalent

Equivalent Grades

DIN 1.4216

Applications

Corrosion-resistant parts, flanges, fasteners

Available Forms

Sheet,Bar,Plate

Uses

Martensitic stainless steel combining moderate corrosion resistance with high strength and hardness after heat treatment. Used for cutlery, surgical instruments, turbine blades, valves, pumps, fasteners and bearings in mildly corrosive environments.

Heat Treatment

Annealing/quench from 980–1050 °C (oil or air) then temper 150–650 °C; lower temper gives higher hardness, higher temper improves toughness.

Precautions

Preheat and post-weld heat treat to avoid hydrogen cracking; soft anneal before heavy machining. Lower corrosion resistance than austenitic grades — not for strong chlorides.