1.4510

Stainless Steel

1.4510

Ti-stabilized ferritic, good weldability. (EN 10088; equiv ASTM 439 / EN 1.4510 / JIS SUS439). Nominal values—confirm mill certificate.

Chemical Composition (%)

C0.07
CR17
TI0.2

Mechanical Properties

Tensile:≥450 MPa;Yield:≥205 MPa

Chinese Standard

EN 10088 1.4510

Equivalent Standards

ASTM 439

Equivalent Grades

EN 1.4510 / JIS SUS439

Applications

钛稳定铁素体,焊接好。,"Sheet

Available Forms

Tube"

Uses

Ferritic stainless steel with good resistance to stress-corrosion cracking and oxidation, plus formability and lower cost. Used for automotive trim, exhaust systems, domestic appliances, decorative and welded structures.

Heat Treatment

Annealed at 780–850 °C and air cooled; stabilize at 600–800 °C to avoid 475 °C embrittlement; not hardenable by heat treatment.

Precautions

Avoid welding in the 475 °C embrittlement and sigma-phase ranges; use matched filler and minimize heat input. Good resistance to stress-corrosion cracking.

Comments 0