1.4662

Stainless Steel

1.4662

Low-Ni duplex, good corrosion resistance. (EN 10088; equiv UNS S82441 / EN 1.4662). Nominal values—confirm mill certificate.

Chemical Composition (%)

C0.03
CR23
NI3
MO0.2
N0.2
MN4

Mechanical Properties

Tensile:≥700 MPa;Yield:≥500 MPa

Chinese Standard

EN 10088 1.4662

Equivalent Grades

UNS S82441 / EN 1.4662

Applications

低镍双相,耐蚀好。,"Plate

Available Forms

Tube"

Uses

Ferritic stainless steel with good resistance to stress-corrosion cracking and oxidation, plus formability and lower cost. Used for automotive trim, exhaust systems, domestic appliances, decorative and welded structures.

Heat Treatment

Annealed at 780–850 °C and air cooled; stabilize at 600–800 °C to avoid 475 °C embrittlement; not hardenable by heat treatment.

Precautions

Avoid welding in the 475 °C embrittlement and sigma-phase ranges; use matched filler and minimize heat input. Good resistance to stress-corrosion cracking.