1010
Alloy Steel1010
(SAE J403). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.09 |
|---|---|
| MN | 0.3 |
| SI | 0.1 |
| P | 0.04 |
| S | 0.05 |
Mechanical Properties
Tensile:≥585 MPa;Yield:≥350 MPa;Elong:≥18%
Equivalent Grades
SAE J403 1010
Available Forms
Bar,Plate
Uses
Low-carbon grade used for welded structures, shafts, pins, bolts, nuts, seamless tubes and general engineering components where moderate strength and good weldability are required. Commonly supplied as bar, plate, sheet, tube and forging.
Heat Treatment
Typically normalized (880–920 °C, air cool) or carburized (900–930 °C) for case-hardening grades, then quenched and tempered at 150–200 °C.
Precautions
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).