1024
Alloy Steel1024
AISI/SAE 1024 carbon / alloy steel.
Chemical Composition (%)
| C | 0.24 |
|---|---|
| MN | 0.3 |
| P | 0.04 |
| S | 0.05 |
Applications
International high-end steel grade for aerospace, oil & gas, defense or engineering machinery.
Available Forms
Bar, plate, sheet, tube, forgings, strip, wire, powder
Uses
Medium-carbon grade for machine parts such as gears, crankshafts, axles, connecting rods, spindles and forgings that need a balance of strength, toughness and machinability. Commonly supplied as bar, plate, sheet, tube and forging.
Heat Treatment
Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.
Precautions
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).