1044
Alloy Steel1044
(AISI/SAE). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.37 |
|---|---|
| MN | 0.3 |
| SI | 0.1 |
| P | 0.04 |
| S | 0.05 |
Mechanical Properties
Tensile:≥585 MPa;Yield:≥350 MPa;Elong:≥18%
Equivalent Grades
SAE 1044
Available Forms
Bar,Plate
Uses
Medium-carbon grade for machine parts such as gears, crankshafts, axles, connecting rods, spindles and forgings that need a balance of strength, toughness and machinability. Commonly supplied as bar, plate, sheet, tube and forging.
Heat Treatment
Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.
Precautions
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).