10Ni-14Co-2Cr
High-Strength10Ni-14Co-2Cr
Secondary-hardening ultra-high-strength steel. (GJB 5255; equiv UNS K92580 / 16Co14Ni10Cr2Mo1). Nominal values—confirm mill certificate.
Chemical Composition (%)
| NI | 9.5 |
|---|---|
| CO | 13.5 |
| CR | 1.8 |
| MO | 0.9 |
| C | 0.13 |
Mechanical Properties
Tensile:≥1515 MPa;Yield:≥1380 MPa
Chinese Standard
GJB 5255 10Ni-14Co-2Cr
Equivalent Grades
UNS K92580 / 16Co14Ni10Cr2Mo1
Applications
二次硬化超高强钢。,"Bar
Available Forms
Forging"
Uses
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈14%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.
Heat Treatment
Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.
Precautions
Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.