1132

Alloy Steel

1132

(SAE J403). Nominal values—confirm mill certificate.

Chemical Composition (%)

C0.27
MN0.6
SI0.1
P0.04
S0.08

Mechanical Properties

Tensile:≥585 MPa;Yield:≥350 MPa;Elong:≥18%

Equivalent Grades

SAE J403 1132

Available Forms

Bar,Plate

Uses

Medium-carbon grade for machine parts such as gears, crankshafts, axles, connecting rods, spindles and forgings that need a balance of strength, toughness and machinability. Commonly supplied as bar, plate, sheet, tube and forging.

Heat Treatment

Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.

Precautions

Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).