12Cr16Ni35

Other

12Cr16Ni35 / S33010 (1Cr16Ni35)

12Cr16Ni35 grade supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

C0.15
SI1.5
MN2
P0.04
S0.03
CR14
NI33

Available Forms

Bar, Plate, Tube, Forging

Uses

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Heat Treatment

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.

Precautions

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.