Alloy Steel15CrMn
Mn quench & temper steel. (GB/T 3077; equiv GB 40Mn2 / DIN 42Mn6). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.38 |
|---|---|
| MN | 1.3 |
Mechanical Properties
Tensile:≥885 MPa;Yield:≥735 MPa
Chinese Standard
T 3077 15CrMn
Equivalent Grades
GB 40Mn2 / DIN 42Mn6
Applications
锰调质钢。,"Bar
Available Forms
Forging"
Uses
Medium-carbon grade for machine parts such as gears, crankshafts, axles, connecting rods, spindles and forgings that need a balance of strength, toughness and machinability. Commonly supplied as bar, plate, sheet, tube and forging.
Heat Treatment
Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.
Precautions
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).