16Cr25Ni20Si2

Other

16Cr25Ni20Si2 / S38340 (1Cr25Ni20Si2)

16Cr25Ni20Si2 grade supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

C0.2
SI1.5
MN1.5
P0.04
S0.03
CR24
NI18

Available Forms

Bar, Plate, Tube, Forging

Uses

Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈19.5%) stabilises the austenite and improves toughness and pitting resistance. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.

Heat Treatment

Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).

Precautions

Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.