2014-T6

Aluminum

2014 aluminum alloy

2014-T6 supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

SI0.5
FE0.7
CU3.9
MN0.4
MG0.2

Equivalent Standards

ASTM B209

Equivalent Grades

Aluminum Association / AA 2014

Applications

Aerospace, automotive, construction, packaging, electrical.

Available Forms

Sheet, Plate, Bar, Extrusion, Foil, Tube, Wire

Uses

Aluminium alloy with good strength-to-weight ratio, corrosion resistance and recyclability. Silicon (≈0.85%) improves castability and lowers thermal expansion. Copper (≈4.45%) raises strength and hardness via precipitation hardening. Used in transport, aerospace, packaging, building and electrical applications.

Heat Treatment

Heat-treatable variants solution treated 470–540 °C and aged (T4/T6); non-heat-treatable grades are strain-hardened. Anneal 340–415 °C.

Precautions

Use sharp, high-rake tooling and appropriate coolants; galling/adhesive wear can occur. Titanium reacts with hydrogen and chlorine — keep out of pickling/HCl environments.