2036-T851
Aluminum2036-T851
Aluminum alloy 2036 (wrought, temper T851).
Chemical Composition (%)
| SI | 0.4 |
|---|---|
| FE | 0.7 |
| CU | 0.15 |
| MN | 0.15 |
| MG | 0.8 |
| CR | 0.04 |
| ZN | 0.25 |
| TI | 0.15 |
Mechanical Properties
Tensile:≥250 MPa;Yield:≥200 MPa;Elongation:≥10%
Equivalent Standards
EN AW
Equivalent Grades
AA 2036
Applications
Aerospace, transport, extrusion
Available Forms
Sheet,Plate,Extrusion
Uses
Aluminium alloy with good strength-to-weight ratio, corrosion resistance and recyclability. Silicon (≈0.6%) improves castability and lowers thermal expansion. Copper (≈0.275%) raises strength and hardness via precipitation hardening. Used in transport, aerospace, packaging, building and electrical applications.
Heat Treatment
Heat-treatable variants solution treated 470–540 °C and aged (T4/T6); non-heat-treatable grades are strain-hardened. Anneal 340–415 °C.
Precautions
Use sharp, high-rake tooling and appropriate coolants; galling/adhesive wear can occur. Titanium reacts with hydrogen and chlorine — keep out of pickling/HCl environments.