2379
Other2379
Cold-work tool steel (DIN 1.2379 / D2).
Chemical Composition (%)
| C | 1.45 |
|---|---|
| SI | 0.1 |
| MN | 0.2 |
| CR | 11 |
| MO | 0.6 |
| V | 0.9 |
| P | 0.03 |
| S | 0.03 |
Applications
High-end / niche grade used in aerospace, defense, tooling, bearing, gear or heavy shaft applications.
Available Forms
Bar, plate, sheet, tube, forgings, strip, wire, powder
Uses
Martensitic stainless steel combining moderate corrosion resistance with high strength and hardness after heat treatment. Used for cutlery, surgical instruments, turbine blades, valves, pumps, fasteners and bearings in mildly corrosive environments.
Heat Treatment
Annealing/quench from 980–1050 °C (oil or air) then temper 150–650 °C; lower temper gives higher hardness, higher temper improves toughness.
Precautions
Preheat and post-weld heat treat to avoid hydrogen cracking; soft anneal before heavy machining. Lower corrosion resistance than austenitic grades — not for strong chlorides.