25 Hot-Rolled Wire

Alloy Steel

25 (Hot-Rolled)

Hot-Rolled 25 Wire for general engineering.

Chemical Composition (%)

C0.22
MN0.5
P0.035
S0.035
SI0.17

Mechanical Properties

Yield:275MPa; Tensile:450MPa; Elong:23%; 125HB

Chinese Standard

GB/T 699

Applications

Shafts, gears, axles, bolts, connecting rods, crankshafts, forgings

Uses

Shafts, gears, axles, connecting rods, bolts, machinery structural parts, automotive and engineering components.

Heat Treatment

Normalized at 850-900°C, air cooled. Quenched + tempered at 550-650°C for improved strength. Specific treatment per grade standard (GB/T 3077, ASTM A29).