2525

Alloy Steel

2525

AISI/SAE 2525 carbon / alloy steel.

Chemical Composition (%)

C0.25
NI4.75
P0.03
S0.03

Applications

International high-end steel grade for aerospace, oil & gas, defense or engineering machinery.

Available Forms

Bar, plate, sheet, tube, forgings, strip, wire, powder

Uses

Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Nickel (≈5%) increases toughness and impact strength at low temperature. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.

Heat Treatment

Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.

Precautions

Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).