25MnTiB
Alloy Steel25MnTiB
Chinese GB steel grade 25MnTiB
Chemical Composition (%)
| C | 0.23 |
|---|---|
| SI | 0.17 |
| MN | 1 |
| CR | 0.3 |
| TI | 0.04 |
| B | 0.0005 |
| P | 0.035 |
| S | 0.035 |
Applications
Chinese national standard (GB) steel grade per GB/T specification.
Available Forms
Bar, plate, sheet, tube, forgings, strip, wire
Uses
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.45%) improves hardenability, wear and corrosion resistance. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.
Heat Treatment
Typically normalized (880–920 °C, air cool) or carburized (900–930 °C) for case-hardening grades, then quenched and tempered at 150–200 °C.
Precautions
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).