2B06

Aluminum

2B06

2B06 grade supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

FE0.3
SI0.2
MN0.4
CU3.8
TI0.1
AL91.8
MG1.7

Available Forms

Bar, Plate, Tube, Forging

Uses

Aluminium alloy with good strength-to-weight ratio, corrosion resistance and recyclability. Silicon (≈0.2%) improves castability and lowers thermal expansion. Copper (≈4.05%) raises strength and hardness via precipitation hardening. Used in transport, aerospace, packaging, building and electrical applications.

Heat Treatment

Heat-treatable variants solution treated 470–540 °C and aged (T4/T6); non-heat-treatable grades are strain-hardened. Anneal 340–415 °C.

Precautions

Use sharp, high-rake tooling and appropriate coolants; galling/adhesive wear can occur. Titanium reacts with hydrogen and chlorine — keep out of pickling/HCl environments.