35ХГСА

Alloy Steel

35ХГСА

Russian GOST silicon-chromium steel.

Chemical Composition (%)

C0.32
SI0.9
MN0.8
CR0.8
P0.025
S0.025

Applications

International high-end steel grade for aerospace, oil & gas, defense or engineering machinery.

Available Forms

Bar, plate, sheet, tube, forgings, strip, wire, powder

Uses

Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.

Heat Treatment

Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.

Precautions

Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).