35Cr Annealed Bar Medium

Alloy Steel

35Cr (Annealed)

Annealed 35Cr Bar Medium for engineering applications.

Chemical Composition (%)

C0.32
CR0.8
MN0.5
SI0.17

Mechanical Properties

Yield:575MPa; Tensile:735MPa; Elong:19%; 215HB

Chinese Standard

GB/T 3077

Applications

Shafts, gears, axles, bolts, connecting rods, crankshafts, forgings

Uses

Shafts, gears, axles, connecting rods, bolts, machinery structural parts, automotive and engineering components.

Heat Treatment

Normalized at 850-900°C, air cooled. Quenched + tempered at 550-650°C for improved strength. Specific treatment per grade standard (GB/T 3077, ASTM A29).