35Mn2
Alloy Steel35Mn2
(GB/T 3077). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.32 |
|---|---|
| SI | 0.17 |
| MN | 1.4 |
| P | 0.035 |
| S | 0.035 |
Mechanical Properties
Tensile:≥835 MPa;Yield:≥685 MPa;Elong:≥12%;RA:≥45%
Chinese Standard
T 3077 35Mn2
Available Forms
Bar,Plate
Uses
Medium-carbon grade for machine parts such as gears, crankshafts, axles, connecting rods, spindles and forgings that need a balance of strength, toughness and machinability. Commonly supplied as bar, plate, sheet, tube and forging.
Heat Treatment
Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.
Precautions
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).