High-Ni, low work-hardening rate. (ASTM A276; equiv ASTM 384 / JIS SUS384). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.08 |
|---|---|
| CR | 15 |
| NI | 17 |
Mechanical Properties
Tensile:≥490 MPa;Yield:≥170 MPa
Chinese Standard
ASTM A276 384
Equivalent Standards
ASTM 384
Equivalent Grades
JIS SUS384
Applications
高镍低加工硬化。,"Wire
Available Forms
Bar"
Uses
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈18%) stabilises the austenite and improves toughness and pitting resistance. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.
Heat Treatment
Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).
Precautions
Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.