4427

Alloy Steel

4427

(AISI/SAE). Nominal values—confirm mill certificate.

Chemical Composition (%)

C0.23
MO0.4
MN0.35
SI0.1
P0.04
S0.05

Mechanical Properties

Tensile:≥585 MPa;Yield:≥350 MPa;Elong:≥18%

Equivalent Grades

SAE 4427

Available Forms

Bar,Plate

Uses

Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Molybdenum (≈0.5%) raises high-temperature strength and prevents temper embrittlement. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.

Heat Treatment

Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.

Precautions

Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).