4626
Alloy Steel4626
(AISI/SAE). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.22 |
|---|---|
| NI | 0.85 |
| MO | 0.2 |
| MN | 0.45 |
| SI | 0.1 |
| P | 0.04 |
| S | 0.05 |
Mechanical Properties
Tensile:≥585 MPa;Yield:≥350 MPa;Elong:≥18%
Equivalent Grades
SAE 4626
Available Forms
Bar,Plate
Uses
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Molybdenum (≈0.25%) raises high-temperature strength and prevents temper embrittlement. Nickel (≈1%) increases toughness and impact strength at low temperature. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.
Heat Treatment
Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.
Precautions
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).