4J335

Other

4J335 / (4J44)

4J335 grade supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

C0.03
SI0.3
MN0.5
P0.02
S0.02
CR0.2
NI34.2
CU0.2

Available Forms

Bar, Plate, Tube, Forging

Uses

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Heat Treatment

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.

Precautions

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.

Comments 0