Alloy Steel5025
(AA 5xxx). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.21 |
|---|---|
| CR | 0.3 |
| MN | 0.6 |
| SI | 0.1 |
| P | 0.04 |
| S | 0.05 |
Mechanical Properties
Tensile:≥585 MPa;Yield:≥350 MPa;Elong:≥18%
Equivalent Grades
AA 5xxx 5025
Available Forms
Bar,Plate
Uses
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.4%) improves hardenability, wear and corrosion resistance. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.
Heat Treatment
Typically normalized (880–920 °C, air cool) or carburized (900–930 °C) for case-hardening grades, then quenched and tempered at 150–200 °C.
Precautions
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).