50W290
Other50W290
Electrical / silicon steel 50W290.
Chemical Composition (%)
| SI | 0.5 |
|---|---|
| C | 0.005 |
| AL | 0.5 |
| MN | 0.3 |
Mechanical Properties
Core loss: low; Flux density: high
Equivalent Standards
Electrical 50W290
Equivalent Grades
IEC
Applications
Transformers, motors, relays
Available Forms
Sheet
Uses
Spring steel with high elastic limit and fatigue strength for coils, leaf springs, clips and suspension parts. Silicon (≈2%) raises elastic limit and tempering resistance. Supplied as strip, wire and bar; shot-peened after forming for longer service life.
Heat Treatment
Austenitize 830–880 °C (oil quench) and temper at 400–520 °C; stress-relieve formed springs at 230–320 °C after coiling.
Precautions
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating). Shot-peen after coiling to improve fatigue life; avoid sharp bends and surface defects.